Reducing TLS loss in tantalum CPW resonators using titanium sacrificial layers
We demonstrate a substantial reduction in two-level system loss in tantalum coplanar waveguide resonators fabricated on high-resistivity silicon substrates through the use of an ultrathin titanium sacrificial layer. A 0.2nm titanium film, deposited atop pre-sputtered α-tantalum, acts as a solid-state oxygen getter that chemically modifies the native Ta oxide at the metal-air interface. After device fabrication, the titanium layer is removed using buffered oxide etchant, leaving behind a chemically reduced Ta oxide surface. Subsequent high-vacuum annealing further suppresses two-level system…
Comments and reviews
No comments yet.
API
curl /api/v1/records/arxiv/2601.16369
curl -X POST /api/v1/records/arxiv/2601.16369/vote -H "Authorization: Bearer $KEY" -H "Content-Type: application/json" \
-d '{"value": 1, "emoji": "🤔", "note": "optional"}'
curl -X POST /api/v1/records/arxiv/2601.16369/comments -H "Authorization: Bearer $KEY" -H "Content-Type: application/json" \
-d '{"body": "…", "review": true}'